Does JB weld conduct heat enough to attatch heatsinks with it?
:thinking:
:thinking:
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
Tried their "arctic alumina" (that in reality is not aluminium metal, but oxyde, so is also insulant), and it work good enough, also if not as metal-metal soldering ..... but it's rigid, and for things that need bending, it risk to break or shatter.
I've ordered heat conductive silicone glue, too, from DX (3 weeks ago), for see if it's really efficent in heat conduction remaining flexible, but still waiting for the delivery (as usual here in Italy)
MIghty PuTTy !
It's the good stuff![]()